Bohler Thermanit 19/15 1.6mm 5kg

Product Description

Bohler Thermanit 19/15 1.6mm 5kg

Stainless; resistant to intercrystalline corrosion and wet corrosion up to 350 °C (662 °F). Corrosion-resistant similar to low-carbon CrNiMo(Mn,N) steels / cast steel grades. Seawater resistant, good resistance to nitric acid, selective attack max. 200 µm. Non magnetic (permeability in field of 8000 A/m 1.01 max.). Particularly suited for corrosion conditions in urea synthesis plants for welding work on steel X2CrNiMo18-12. Well suited for joining and surfacing applications with matching and similar austenitic CrNi(N) and CrNiMo(Mn,N) steels / cast steel grades.

Technical Specifications

Classifications

EN ISO 14343-AW 20 16 3 Mn N L
AWS A5.9ER316LMn
Mat. No.1.4455